Notes: Monprene CP-18200 Unfilled, High Flow Series of thermoplastic elastomer compounds, with good UV resistance, available in NAT or colors, from 40 to 80 Shore A, are designed specifically for EU consumer product applications requiring a soft, rubber-like feel. Monprene CP-18270 is a medium hardness, low density grade that is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Toughness; High Flow; Low Density; Low Specific Gravity; Medium Hardness; UV Resistant; Without Fillers Uses: Bushings; Consumer Applications; Flexible Grips; Gaskets; General Purpose; Grommets; Handles; Knobs; Luggage; Overmolding; Plugs; Rubber Replacement; Soft Touch Applications RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |