MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Chockfast® Super Ceramic Repair Putty Ceramic Filled Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: SUPER CERAMIC Repair Putty is a smooth ceramic-filled epoxy putty with exceptional wear resistance. The "no-slump" nature of SUPER CERAMIC Repair Putty makes it ideal for repairing overhead, vertical or curved surfaces.

USE & BENEFITS: SUPER CERAMIC Repair Putty is well suited for the repair of "severe service" pump equipment commonly found in industries, such as pulp and paper mills, chemical processing, refineries, marine and coal mining operations as well as many others.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D1700
Compressive Strength 87.6 MPa12700 psiASTM D695
Adhesive Bond Strength 12.4 MPa1800 psiAdhesive Tensile Shear; ASTM D1002
Izod Impact, Notched 0.149 J/cm0.280 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 44.6 µm/m-°C24.8 µin/in-°FASTM D698
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 22.0 °C
24.0 hour
@Temperature 71.6 °F
approximate
Pot Life 20.0 min
@Temperature 22.2 °C
20.0 min
@Temperature 72.0 °F
 
Descriptive Properties
Colorgrayresin
 white, grayhardener, after mixing
Mix Ratio by volume4.3 to 1
Mix Ratio by weight7 to 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9029 / 239539

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.