MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen GM 9240 HT High Density Polyethylene (HDPE), Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Hostalen GM 9240 HT is a high density polyethylene characterized by superior toughness and stiffness. Hostalen GM 9240 HT can be converted on HDPE blown film equipment with a homogeneous appearance and very low gel level. The very good bubble stability permits the production of wrinkle free and flat films within a wide range of blow up ratios. Typical applications are carrier and meat bags, inliners for drums, paper bags and FIBC as well as heavy duty bags. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Heavy Duty Packaging, Lamination Film, Liner Film, Products for Use in Property Modification

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.946 g/ccISO 1183-1
Melt Flow 0.17 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 6.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 475 %ISO 527-1,-3
Film Elongation at Break, TD 400 %ISO 527-1,-3
Dart Drop Test >= 150 g
Film Tensile Strength at Break, MD 64.0 MPaISO 527-1,-3
Film Tensile Strength at Break, TD 60.0 MPaISO 527-1,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 230 °C
 
Descriptive Properties
Processing MethodBlown Film
Test Specimenfilm, 20µm blown film extruded at 220°C, long stalk process, and a blow up ratio 4:1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen ACP 9254 Plus High Density Polyethylene (HDPE), Film Grade
LyondellBasell Hostalen GF 9055 F High Density Polyethylene (HDPE), Film Grade
LyondellBasell Hostalen GF 7750 M2 High Density Polyethylene (HDPE), Film Grade
LyondellBasell Hostalen GM 5010 T3 S RED High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
LyondellBasell Hostalen GD 9550 F High Density Polyethylene (HDPE), Film Grade

PEQT8495 / 220130

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.