MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Durez 32633 Black Phenolic is a two-stage, glass filled, special purpose molding compound. It is designed for applications requiring high physical strengths, dimensional stability, and heat resistance. Typical applications include small motor and gear housings, brush holders, commutators, and under hood automotive applications.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.78 g/cc0.0643 lb/in³ASTM D792
Apparent Bulk Density 0.800 g/cc0.0289 lb/in³ASTM D1895
Water Absorption 0.050 %0.050 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 138 MPa20000 psiASTM D638
Tensile Modulus 18.6 GPa2700 ksiASTM D638
Flexural Strength 227 MPa32900 psi
Flexural Modulus 15.2 GPa2200 ksi
Compressive Strength 276 MPa40000 psiASTM D695
Compressive Modulus 10.5 GPa1530 ksi@ 250°F
Shear Strength 47.4 MPa6870 psi
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmASTM D257
Dielectric Constant  4.3
@Frequency 1e+6 Hz
4.3
@Frequency 1e+6 Hz
ASTM D150
 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
ASTM D150
 4.4
@Frequency 1000 Hz
4.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm399 kV/inStep by step; ASTM D149
 17.7 kV/mm450 kV/inShort Time; ASTM D149
Dissipation Factor  0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
 0.030
@Frequency 60 Hz
0.030
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C
@Thickness 3.00 mm
302 °F
@Thickness 0.118 in
Deflection Temperature at 1.8 MPa (264 psi) 204 °C399 °FASTM D648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 6.00 mm
V-0
@Thickness 0.236 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Compression Grade
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 156 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 31735 Phenolic, Injection Grade
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade

P90X55 / 21172

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.