MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cracking resistance. When compared to LDPE grades of equivalent density, LL 6301 grades exhibits a higher heat deflection temperature and a significantly greater resistance to long term creep.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Caps
  • Housewares
  • Technical Parts
  • Threaded Closures

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.936 g/cc0.0338 lb/in³ExxonMobil method
ESCR 10% Igepal® 30 hour
@Temperature 50.0 °C
30 hour
@Temperature 122 °F
ASTM D1693B
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 13.8 MPa2000 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Elongation at Yield 20 %20 %ASTM D638
Flexural Modulus, 1% Secant 490 MPa71000 psiASTM D790
Izod Impact, Notched (ISO) 39.9 kJ/m²19.0 ft-lb/in²ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 125 °C<= 257 °FPeak Melting Point; ExxonMobil method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LLDPE LL 6201XR Molding Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 6201RQ Molding Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 8446.21 Linear Low Density Polyethylene Resin (European Grade)
ExxonMobil LLDPE LL 1001XV Wire & Cable Linear Low Density Polyethylene Resin (European Grade)

PEX99196 / 175432

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.