MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubriplate NO.8 Petroleum-Based Machine Tool Oil
Categories: Fluid; Lubricant

Material Notes: Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity.

Machine Tool Oils are available in Bottles, Jugs, Pails, 1/4 Drums & Drums.

Information provided by Lubriplate

Key Words: Part Number L0014-
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9090Viscosity Index
 460460ISO Grade
Saybolt Viscosity at 100°F 2300 SUS2300 SUS
Saybolt Viscosity at 210°F 142 SUS142 SUS
Kinematic Viscosity at 40°C (104°F) 432 cSt432 cSt
Kinematic Viscosity at 100°C (212°F) 28 cSt28 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -17.8 °C0.000 °F
Flammability Test 515515[°F] Fire Point
Flash Point 224 °C435 °F
 
Descriptive Properties
SAE Gear Oil No.140
SAE No.70

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WLUBR108 / 76154

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.