Features: Good balance of flow, strength and set-up properties. Applications: Consumer electronic packaging Data provided by the manufacturer. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |