This is a general purpose injection molding grade thermoplastic elastomer based on SEBS technology. It is suitable for food contact applications. Physical Form: Pellet. Standard Color: Off white, opaque. Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. |