MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography  (discontinued **)
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Epoxy

Material Notes: Description

DSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially useful in applications requiring optical clarity such as fluid flow analysis, stress analysis and light pipes. Other applications include those that require a strong and durable product without the brittleness normally associated with a rigid stereolithography resin.

Application

Somos® 10110 Photopolymer is used in the solid imaging process to build three-dimensional parts. Somos® 10110 requires a minimal post-cure by UV fluorescent light. Prolonged exposure to UV light will create a yellow tinge to the parts.

Information Provided by DSM Desotech Inc.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.


Axis Proto Inc. North American leaders for providing high quality Rapid Prototyping and Rapid Manufacturing solutions using all major Additive systems including Stereolithography printing. Free 3D printing quotes at www.axisproto.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc
@Temperature 25.0 °C
0.0405 lb/in³
@Temperature 77.0 °F
Water Absorption 0.98 %0.98 %ASTM D570-98
Viscosity 130 cP
@Temperature 30.0 °C
130 cP
@Temperature 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ASTM D2240
Tensile Strength, Yield 43.4 MPa6290 psiASTM D638M
Elongation at Break 37 %37 %ASTM D638M
Elongation at Yield 4.2 %4.2 %ASTM D638M
Modulus of Elasticity 2.04 GPa296 ksiASTM D638M
Flexural Strength 57.7 MPa8370 psiASTM D790M
Flexural Modulus 1.72 GPa249 ksiASTM D790M
Poissons Ratio 0.360.36ASTM D638M
Shear Modulus 0.750 GPa109 ksiCalculated
Izod Impact, Notched 0.450 J/cm0.843 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150-98
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150-98
 3.9
@Frequency 60.0 Hz
3.9
@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 15.3 kV/mm389 kV/inASTM D149-97a
 
Thermal PropertiesMetricEnglishComments
CTE, linear  75.9 µm/m-°C
@Temperature -40.0 - 0.000 °C
42.2 µin/in-°F
@Temperature -40.0 - 32.0 °F
ASTM E831-00
 109.2 µm/m-°C
@Temperature 0.000 - 50.0 °C
60.67 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E831-00
 161 µm/m-°C
@Temperature 50.0 - 100 °C
89.4 µin/in-°F
@Temperature 122 - 212 °F
ASTM E831-00
 183 µm/m-°C
@Temperature 100 - 150 °C
102 µin/in-°F
@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 51.2 °C124 °FASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 44.9 °C113 °FASTM D648-98c
Glass Transition Temp, Tg 41.0 °C106 °FASTM E1545-00
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.511.51ASTM D542-00
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
AppearanceOptically Clear
Dp (mm)0.146Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2)51Exposure that gives 0.254mm thickness
Ec (mJ/cm2)9Critical exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin
DSM Somos® NanoForm™ 15120 Nanocomposite Resin for Stereolithography, UV Postcure
DSM Somos® NanoForm™ 15120 Nanocomposite Resin for Stereolithography, UV & Thermal Postcure

PDSMT024 / 93544

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.