MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Schweitzer-Mauduit Argotec™ 46510 WHITE Polycaprolactone-based aliphatic polyurethane (TPU)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Graphic Film 46510 CLEAR. Polycaprolactone-based aliphatic polyurethane (TPU).

Applications: Premium performance graphic film over laminate face stock.

Attributes: Class A gloss finish, Highly conformable, Excellent abrasion resistance, Excellent low-temperature flexibility & cold-crack resistance, UV resistant (5 year outdoor durability), No additives-consistent, excellent adhesive compatibility/anchorage, Halogen free.

Information provided by Schweitzer-Mauduit International, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 - 102 microns1.00 - 4.00 mil
Surface Tension >= 35 dynes/cm>= 35 dynes/cmASTM D-2578
 
Mechanical PropertiesMetricEnglishComments
Elongation, Ultimate 450 %450 %ASTM D-412
100% Modulus 48.3 MPa7000 psiASTM D-412
Taber Abrasion, mg/1000 Cycles <= 3.5<= 3.5C-17 Wheel, 1000 gram weight; ASTM D1044
 
Optical PropertiesMetricEnglishComments
Gloss >= 80 %>= 80 %@ 60°; OTM 3-309
 
Descriptive Properties
AppearanceWhite
LengthUp to 1000 non-spliced yards
UV ResistanceChange in Yellowness Index (YI) <1.5 at 2000 hrsASTM D-4329 cycle B
WidthUp to 62"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCHWE907a / 287668

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.