MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik REWOTERIC® AM 2 C NM Foam booster
Categories: Fluid

Material Notes: Product description: N-coconut fatty acid amidoethyl-N-hydroxyethyl glycinate.

Application: REWOTERIC AM 2 C NM may be used as foam booster. It may be also used as coupler or wetting agent in cleaning surfactant systems.

Properties / Benefits: REWOTERIC® AM 2 C NM is an amphoteric surfactant which is stable to alkaline and acidic conditions. It is compatible with cationic, amphoteric, anionic and other non-ionic products. REWOTERIC® AM 2 C NM has good foaming properties even in the presence of oil or soap. It is a very good lime soap dispersant and wetting agent. REWOTERIC® AM 2 C NM has high resistance to hard water.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 49 - 51 %
pH 8.0 - 8.612% in water
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0
 
Descriptive Properties
Appearanceyellow, clear liquid
Content>39%Actives
 9-10%NaCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTANAT® TMDI Diisocyanate

PEVONIL531 / 196735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.