MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
AGC Fluon® FC 15 MIN SPL PTFE, 15% Wollastonite Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Fluon® FC 15 MIN SPL (340 454 463) is a 15% wollastonite–filled PTFE product designed for use in seal applications. This compound is supplied in round pelletized form. These pellets range in size from approximately 350 – 800 microns.

End Uses: Wollastonite fibers are added to PTFE to improve the wear properties, abrasion, compressive strength, and creep resistance of PTFE without sacrificing the chemical and thermal resistance of the polymer.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.19 g/ccASTM D4745
Bulk Density 0.800 g/ccASTM D4894
Filler Content 15 %ASTM D4745
Linear Mold Shrinkage 0.024 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59Sustained; ASTM D2240
 61Peak; ASTM D2240
Tensile Strength 3100 psiASTM D4745
Elongation at Break 250 %ASTM D4745

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
AGC Fluon® FC 15 MIN PTFE, 15% Wollastonite Filled
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
Rogers Arlon CLTE-XT High Precision Ceramic PTFE

PAGCX102 / 191211

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.