MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LEXAN™ Copolymer XHT3141 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.300 %0.300 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %0.30 %ISO 62-1
Viscosity 30 cP
@Load 2.16 kg,
Temperature 330 °C
30 cP
@Load 4.76 lb,
Temperature 626 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 330 °C
33 g/10 min
@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.0 MPa7980 psi50 mm/min; ASTM D638
 60.0 MPa8700 psi50 mm/min; ISO 527
Tensile Strength, Yield 70.0 MPa10200 psi50 mm/min; ASTM D638
 70.0 MPa10200 psi50 mm/min; ISO 527
Elongation at Break 70 %70 %50 mm/min; ASTM D638
 70 %70 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.50 GPa363 ksi1 mm/min; ISO 527
 2.70 GPa392 ksi5 mm/min; ASTM D638
Flexural Strength 80.0 MPa11600 psiyield, 2 mm/min; ISO 178
 120 MPa17400 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
 2.60 GPa377 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 97.0 J71.5 ft-lbASTM D256
 55.0 J
@Temperature -30.0 °C
40.6 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*3; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 68.0 J50.2 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+17 ohm-cm>= 1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant  2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
ASTM D150
 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
ASTM D150
Dielectric Strength 23.0 kV/mm
@Thickness 3.20 mm
584 kV/in
@Thickness 0.126 in
in oil; ASTM D149
Dissipation Factor  0.011
@Frequency 1e+6 Hz
0.011
@Frequency 1e+6 Hz
ASTM D150
 0.031
@Frequency 100 Hz
0.031
@Frequency 100 Hz
ASTM D150
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness 1.50 mm
15 - 30 sec
@Thickness 0.0591 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 164 °C327 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 166 °C
@Thickness 3.20 mm
331 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 156 °C
@Thickness 3.20 mm
313 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 168 °C334 °FRate B/50; ISO 306
 170 °C338 °FRate B/50; ASTM D1525
 170 °C338 °FRate B/120; ISO 306
UL RTI, Electrical 150 °C302 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 150 °C302 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Glow Wire Ignition Temperature 875 °C
@Thickness 3.00 mm
1610 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 285 - 345 °C545 - 653 °F
Zone 2 280 - 340 °C536 - 644 °F
Zone 3 290 - 350 °C554 - 662 °F
Melt Temperature 290 - 350 °C554 - 662 °FInjection Molding
Mold Temperature 95.0 - 130 °C203 - 266 °F
Drying Temperature 135 °C275 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00800 cm0.000984 - 0.00315 in
Screw Speed 40 - 90 rpm40 - 90 rpm
 
Descriptive Properties
Metallized Haze Onset165 °CSABIC method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80452 / 288399

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.