MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Polyhydroxybutyrate / Polyhydroxyvalerate (PHB 92/PHV 8)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic

Material Notes: See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents of 5 - 20% give a useful range of properties broadly similar to those of the polyolefins (the polyethylenes and polypropylene). They melt at lower temperatures than the homopolymer, giving a useful improvement in melt-processability. Their other properties are similar to those of PHB.

They are being used for biodegradable containers (of which shampoo bottles are the most high-profile example) and other articles difficult to recycle e.g. disposable razors or medically contaminated articles.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 25.0 - 30.0 MPa
Film Tensile Strength at Yield, TD 25.0 - 30.0 MPa
Tensile Strength, Yield 28.0 MPa
Film Elongation at Break, MD 7.0 - 15 %
Film Elongation at Break, TD 5.0 - 10 %
Elongation at Break 15 %
Tensile Modulus 0.900 GPa
Secant Modulus, MD 0.600 - 1.00 GPaFilm
Secant Modulus, TD 0.800 - 1.20 GPaFilm
Izod Impact, Unnotched 1.00 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.40 J/g-°C
Thermal Conductivity 0.150 W/m-K
 
Descriptive Properties
Chemical Resistance - AlcoholsFair
Chemical Resistance - AlkalisPoor
Chemical Resistance - Dilute AcidsFair
Chemical Resistance - Greases and OilsGood
Permeability to Oxygen @25°C0.1-0.2 x 10-13 cm3.cm cm-2 s-1 Pa -1Film
Permeability to Water @25°C1000-2000 x 10-13 cm3.cm cm-2 s-1 Pa -1Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Polyhydroxybutyrate - Biopolymer PHB
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12)
Biomer P304 PHB Biodegradable Polymer
Biomer P209 PHB Biodegradable Polymer
Reliance Industries METABOLIX PHB

PGOODF219 / 42290

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.