MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TSRC T-BLEND® 1001-45C TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermoplastic rubber compound materials produced by TSRC CORPORATION. T-BLEND® 1001-45C is a pre-formulated and pelletized thermoplastic elastomer compound based on styrenic block copolymer. It is designed for the injection molding of non-toxic toy components and insole product parts. It has the smooth surface and the clear appearance. It is very suitable to apply in manufacturing soft product and get the comfortable touch feeling. Being a thermoplastic elastomer, T-BLEND® 1001-45C can be easily processed with general processing equipment and tools designed for thermoplastics and yet possess elastomeric properties at ambient temperatures.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 - 0.950 g/cc0.890 - 0.950 g/ccASTM D792
Linear Mold Shrinkage 0.020 - 0.025 cm/cm0.020 - 0.025 in/in
Melt Flow 10 - 30 g/10 min
@Load 8.00 kg,
Temperature 180 °C
10 - 30 g/10 min
@Load 17.6 lb,
Temperature 356 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 42 - 4842 - 48ASTM D2240
Tensile Strength 6.08 MPa882 psiType3, specimen; ASTM D412
Elongation at Break 986 %986 %500 mm/min; ASTM D412
300% Modulus 2.65 MPa384 psi500mm/min; ASTM D412
Tear Strength 30.4 kN/m174 pliC Die; ASTM D624
 
Processing PropertiesMetricEnglishComments
Feed Temperature 150 °C302 °F
Rear Barrel Temperature 170 °C338 °F
Front Barrel Temperature 160 °C320 °F
Nozzle Temperature 180 °C356 °F
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
Cycle Time - Injection 60 - 80 sec60 - 80 sec
 
Descriptive Properties
ColorTranslucent
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC043 / 306331

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.