Sandvik 2RK65 is an austenitic stainless ELC steel intended for use under severe corrosion conditions within the process industry. The material is characterized by the following properties: very good resistance to attacks in acidic environments, e.g. sulphuric, phosphoric and acetic acid very good resistance to pitting in neutral chloride-bearing solutionsmuch better resistance to crevice corrosion than steels of the AISI 304 and AISI 316 type very good resistance to stress corrosion crackinggood weldability Information provided by Sandvik UNS N08904; EN 1.4539 |