MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Indium Corp. Indalloy® 117 Bi-Pb-In-Sn-Cd Fusible Alloy
Categories: Metal; Nonferrous Metal; Lead Alloy

Material Notes: General purpose fusible alloy.

Information Provided by Indium Corporation

Key Words: Other trade names: Cerrolow 117
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.16 g/cc0.331 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 16.5
@Load 4.00 kg
16.5
@Load 8.82 lb
2mm ball
Tensile Strength, Ultimate 37.2 MPa5400 psi
Elongation at Break 37.5 %37.5 %% elongation on 5.65 (sq. root Area) gauge length
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000380 ohm-cm0.0000380 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 36.8 J/g15.8 BTU/lb
CTE, linear 25.0 µm/m-°C
@Temperature 20.0 °C
13.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.163 J/g-°C0.0390 BTU/lb-°FSolid
 0.197 J/g-°C0.0471 BTU/lb-°FLiquid
Thermal Conductivity 15.0 W/m-K
@Temperature 85.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 185 °F
Melting Point 47.0 °C117 °FEutectic
Solidus 47.0 °C117 °F
Liquidus 47.0 °C117 °F
 
Component Elements PropertiesMetricEnglishComments
Bismuth, Bi 44.7 %44.7 %
Cadmium, Cd 5.3 %5.3 %
Indium, In 19.1 %19.1 %
Lead, Pb 22.6 %22.6 %
Tin, Sn 8.3 %8.3 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 136 Bi-In-Pb-Sn Fusible Alloy
AIM 47 Fusible Bismuth Alloy
Indium Corp. Indalloy® 19 In-Bi-Sn Fusible Alloy
Indium Corp. Indalloy 157 Lead Solder Alloy
AIM 58 Fusible Alloy

NNIN03 / 18459

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.