MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes:

All information provided by Wellman Engineered Resins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183-87
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cmDIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cmDIS 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPaISO 527-93
Elongation at Break 3.0 %ISO 527-93
Flexural Strength 165 MPaISO 178-93
Flexural Modulus 7100 MPaISO 178-93
Izod Impact, Notched (ISO) 6.00 kJ/m²ISO 180-93
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 240 °CISO 75-93
Flammability, UL94 V-0
@Thickness 0.800 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epsan Eplamid 66 GX0 25 RP Q1C5B601 Polyamide 66, Halogen Free
Domo Technyl® A 60G1 V25 25% Glass Reinforced Nylon 66, Flame Retardant
Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
LATI Latamid 66 H2 G/25-V0CT1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Ravago Manufacturing Americas Hylon® N1025HLFRA Nylon 66, 25% Glass Filled, Conditioned

PWEL00153 / 88073

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.