MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TROGAMID® eCO myCX BC100 I Microcrystalline, permanently transparent polyamide, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: TROGAMID® eCO myCX BC100 I is a microcrystalline transparent polyamide for the manufacture of parts in the optical industry, like lenses, by injection molding. eCO stands for Evoniks aim to eliminate CO2 through use of renewable or circular feedstocks via massbalance approach. TROGAMID® eCO myCX BC100 I is supplied as spherical pellets in moisture-proof packaging. Preliminary data sheet.
Industrial Sector: Sustainable, Optics, Sports and Lifestyle
Sustainability: eCO
Processing: Injection molding , Extrusion
Optics: Transparent, High gloss, X-ray transparent
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Fatigue resistance
Conformity: Food contact
Additives: Unfilled
Applications: Fiber optic cable, (Sun-) glasses, Hygiene and cosmetics, Lenses, Monofilament
Processing: Film extrusion
Special Characteristics: Halogen-free, Phosphorus-free, High impact strength, Low viscosity
Features: optical UV-protection, Weldable, Low birefringence, Non-corrosive, Dishwasher detergents resistant
Regulatory: Food contact 10/2011/EC
Color: Natural color
Delivery form: Spherical pellets

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527
Tensile Strength 63.0 MPaISO 527
Tensile Stress 39.0 MPa
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 63.0 MPaISO 527
Elongation at Break 185 %Nominal; ISO 527
Elongation at Yield 7.00 %ISO 527
Tensile Modulus 1490 MPaISO 527
Flexural Strength 54.0 MPaat conv. Deflection; ISO 178
 88.0 MPaISO 178
Flexural Modulus 1500 MPaISO 178
Flexural Strain at Break 8.00 %at flexural strength; ISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
Type of failure: C; ISO 179/1eA
 12.0 kJ/m²
@Temperature -40.0 °C
Type of failure: C; ISO 179/1eA
 
Descriptive Properties
Blue water consumption18 kgISO 14040, 14044
ColorNatural Color
Global Warming Potential2.5 kg CO2 eq./kgincl. bio. C incl. LUC, ISO 14040, 14044
 5.3 kg CO2 eq./kgexcl. bio. C incl. LUC, ISO 14040, 14044
Land use (ReCiPe 2016)1.0 Annual crop eq. yISO 14040, 14044

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK7829 / 324961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.