Kaowool Rigidizer is a colloidal silica compound for treating surfaces of Kaowool ceramic fiber products to provide a degree of surface hardness and resistance to erosion. Kaowool Rigidizer is stabilized against freezing during exposure to cold; however, freezing should be avoided. Features: Increases surface hardness and resistance to erosion Easily applied by brushing or spraying Freeze resistant Applications: Surface coating for Kaowool ceramic fiber blanket exposed to high velocity gases Adhesive for use in making composites and laminates Surface treatment for Kaowool vacuum formed shapes to increase surface hardnessInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |