MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Precipitation Hardening Stainless
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Precipitation Hardening Stainless". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.50 - 7.90 g/ccAverage value: 7.76 g/cc Grade Count:137
Porosity 0.000 - 4.00 %Average value: 3.00 % Grade Count:4
Particle Size 6.70 - 12.0 µmAverage value: 9.27 µm Grade Count:12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 255 - 567Average value: 362 Grade Count:47
Hardness, Knoop 265 - 631Average value: 408 Grade Count:39
Hardness, Rockwell B 80.0 - 105Average value: 95.8 Grade Count:25
Hardness, Rockwell C 20.0 - 55.5Average value: 38.0 Grade Count:108
Hardness, Vickers 153 - 604Average value: 382 Grade Count:41
Tensile Strength, Ultimate 120 - 3100 MPaAverage value: 1280 MPa Grade Count:145
Tensile Strength, Yield 255 - 2500 MPaAverage value: 1090 MPa Grade Count:145
Elongation at Break 0.000 - 70.0 %Average value: 12.2 % Grade Count:136
Elongation at Yield 0.000 - 18.0 %Average value: 12.1 % Grade Count:3
Reduction of Area 10.0 - 76.0 %Average value: 45.7 % Grade Count:36
Modulus of Elasticity 77.0 - 230 GPaAverage value: 194 GPa Grade Count:98
Poissons Ratio 0.270 - 0.300Average value: 0.275 Grade Count:16
Machinability 35.0 - 60.0 %Average value: 39.0 % Grade Count:8
Shear Modulus 68.9 - 77.4 GPaAverage value: 75.6 GPa Grade Count:15
Charpy Impact 6.00 - 236 JAverage value: 65.6 J Grade Count:39
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000769 - 0.000100 ohm-cmAverage value: 0.0000832 ohm-cm Grade Count:53
Magnetic Permeability 1.40 - 208Average value: 87.8 Grade Count:22
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 - 16.9 µm/m-°CAverage value: 11.1 µm/m-°C Grade Count:84
Specific Heat Capacity 0.419 - 0.490 J/g-°CAverage value: 0.442 J/g-°C Grade Count:50
Thermal Conductivity 12.9 - 34.3 W/m-KAverage value: 16.2 W/m-K Grade Count:10
Melting Point 1400 - 1470 °CAverage value: 1430 °C Grade Count:38
Solidus 1400 - 1410 °CAverage value: 1400 °C Grade Count:38
Liquidus 1440 - 1470 °CAverage value: 1450 °C Grade Count:38
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.100 - 1.60 %Average value: 1.05 % Grade Count:70
Carbon, C 0.0100 - 0.200 %Average value: 0.0615 % Grade Count:156
Chromium, Cr 0.250 - 52.0 %Average value: 16.1 % Grade Count:160
Copper, Cu 2.00 - 14.0 %Average value: 4.02 % Grade Count:96
Iron, Fe 23.8 - 93.4 %Average value: 73.1 % Grade Count:160
Manganese, Mn 0.100 - 2.00 %Average value: 0.873 % Grade Count:150
Molybdenum, Mo 0.300 - 4.00 %Average value: 2.24 % Grade Count:51
Nb + Ta 0.150 - 0.450 %Average value: 0.297 % Grade Count:57
Nickel, Ni 3.00 - 14.0 %Average value: 5.91 % Grade Count:160
Niobium, Nb (Columbium, Cb) 0.150 - 0.900 %Average value: 0.364 % Grade Count:39
Nitrogen, N 0.00500 - 0.900 %Average value: 0.250 % Grade Count:15
Oxygen, O 0.250 %Average value: 0.250 % Grade Count:4
Phosphorus, P 0.00500 - 0.0450 %Average value: 0.0301 % Grade Count:125
Silicon, Si 0.0500 - 3.00 %Average value: 0.891 % Grade Count:144
Sulfur, S 0.00400 - 0.0800 %Average value: 0.0240 % Grade Count:126
Tantalum, Ta 0.0500 - 0.450 %Average value: 0.389 % Grade Count:9
Titanium, Ti 0.0100 - 0.900 %Average value: 0.307 % Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for T 300 Series Stainless Steel
Overview of materials for T 400 Series Stainless Steel
Overview of materials for T S10000 Series Stainless Steel
303 Stainless Steel, annealed
Overview of materials for Stainless Steel

M01023 / 81733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.