MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Avient LubriOne™ NN-30CF/15T Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 193 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 12400 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 276 MPaASTM D790
Flexural Modulus 12400 MPaASTM D790
Izod Impact, Notched 123 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HBUL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 288 - 299 °C
Mold Temperature 82.2 - 93.3 °C
Drying Temperature 71.1 - 82.2 °C
@Time 7200 sec
 
Descriptive Properties
FeaturesLubricated
FormsPellets
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAppliance Components
 Conveyor Parts
 Printer Parts

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kuraray Genestar™ G1301A-M61 Nylon, 30% Glass Filled
Avient LubriOne™ NN-000/20T Polyamide 66 (Nylon 66)
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber
Kuraray Genestar™ G1352A-M41 Nylon, 35% Glass Filled
Avient LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66)

PH1PN9086 / 102922

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.