MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shandong Dongyue Shenzhou New Material Co 3-methoxy-2,2,3,3-tetrafluoropropionatemethylester (MTPME)
Categories: Other Engineering Material

Material Notes: Conformable with: Q/DYS 009-2007

MTPME is a kind of transparent liquid, aromatic, flammable, stable, nontoxic, easy to decompose at high temperature. It is not only the key intermediate for synthesis of fluorine-containing ether and carboxyl resin, but also a kind of solvent.

Main Applications:

MTPME is one important intermediate of perfluorocarboxylic resin and raw material of fluoride vinyl ether. It can also be used to prepare adhesion agent, dyestuff, medicine intermediate and polymer. MTPME is also a kind of solvent.

Information Provided by Shandong Dongyue Shenzhou New Material Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc
@Temperature 25.0 °C
0.0520 lb/in³
@Temperature 77.0 °F
Liquid
Molecular Weight 190 g/mol190 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point 150 °C
@Pressure 0.1013 MPa
302 °F
@Pressure 14.69 psi
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Descriptive Properties
Chemical Name3-methoxy-2,2,3,3-tetrafluoropropionatemethylester
Danger Label3 (flammable)
Molecular FormulaCH3OCF2CF2COOCH3
Purity (%)>95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSHEN008 / 104063

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.