MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LyondellBasell Petrothene® NA480178 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low temperature flexibility. Applications include ice bags, frozen food packaging, bundling and heavy-duty bags.

Regulatory Status
NA 480 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
NA 480 has been designed to provide excellent processability over a wide range of extrusion conditions. However, optimum properties are produced at temperatures of 330°-430°F with a blow-up ratio between 1.7-4.0:1. Drawdown to 1.25 mils is not uncommon at commercial rates when proper

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Vinyl Acetate Content 4.5 %4.5 %
Thickness 50.8 microns2.00 mil2:1 BUR; 25 mil die gap
Melt Flow 0.25 g/10 min0.25 g/10 minASTM D1238
Slip Level 0.000 ppm0.000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 370 %370 %ASTM D882
Film Elongation at Break, TD 550 %550 %ASTM D882
Elmendorf Tear Strength MD 150 g150 gASTM D1922
Elmendorf Tear Strength TD 250 g250 gASTM D1922
Dart Drop Test 320 g0.706 lbF50; ASTM D1709
Film Tensile Strength at Break, MD 22.1 MPa3200 psiASTM D882
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D882
1% Secant Modulus, MD 131 MPa19000 psiASTM D882
1% Secant Modulus, TD 159 MPa23000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 °C430 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntiblockHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQU0493c / 36952

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.