MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Titanium Ti-6Al-2Nb-1Ta-1Mo, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Annealed 700-870°C for 15 - 120 min.

Characteristics: High toughness, moderate strength, weldability, resistance to seawater corrosion, unheat-treatable.

Applications: Marine and sub-marine vehicles - hardware and hull structures, Naval aircraft.

Forms available: Billet, bar and plate.

1 other heat treatment of this alloy is in MatWeb.

Key Words: Ti6Al2Nb1Ta1Mo, Ti-6211; Ti-621/0.8; UNS R56210
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.48 g/cc0.162 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 290290Estimated from Rockwell C.
Hardness, Knoop 315315Estimated from Rockwell C.
Hardness, Rockwell C 3030
Hardness, Vickers 304304Estimated from Rockwell C.
Tensile Strength 586 MPa
@Temperature 427 °C
85000 psi
@Temperature 801 °F
Tensile Strength, Ultimate 860 MPa125000 psi
Tensile Strength, Yield 760 MPa110000 psi
Elongation at Break 14 %14 %
Tensile Modulus 115.8 GPa16800 ksi
Modulus of Rigidity 24.0 GPa3480 ksi
Compressive Yield Strength 790 MPa115000 psi
Compressive Modulus 124 GPa18000 ksi
Notched Tensile Strength 1210 MPa175000 psiKt (stress concentration factor) = 5.8
Poissons Ratio 0.310.31Typical for alpha titanium alloy.
Fatigue Strength  170 MPa
@# of Cycles 1.00e+7
24700 psi
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 3.0
 280 MPa
@# of Cycles 1.00e+7
40600 psi
@# of Cycles 1.00e+7
unnotched
Fracture Toughness 100 MPa-m½91.0 ksi-in½KIC
Shear Modulus 44.2 GPa6410 ksiCalculated from typical values.
Shear Strength 580 MPa84100 psiUltimate shear strength
Charpy Impact 54.0 J39.8 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000154 ohm-cm0.000154 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.20 µm/m-°C
@Temperature 20.0 - 93.0 °C
5.11 µin/in-°F
@Temperature 68.0 - 199 °F
Specific Heat Capacity 0.550 J/g-°C0.131 BTU/lb-°FEstimated from similar materials
Thermal Conductivity 6.40 W/m-K44.4 BTU-in/hr-ft²-°F
Melting Point <= 1650 °C<= 3000 °FEstimated from similar materials
Liquidus 1650 °C3000 °FEstimated from similar materials
Beta Transus 1016 °C1861 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 6.0 %6.0 %
Molybdenum, Mo 1.0 %1.0 %
Niobium, Nb (Columbium, Cb) 2.0 %2.0 %
Tantalum, Ta 1.0 %1.0 %
Titanium, Ti 90 %90 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Nb-1Ta-1Mo
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), Alpha-Annealed
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), STA
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), STA-1
Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), as-rolled

MTA612 / 14131

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.