MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toyobo VYLOPET® EMC618P PBT/PET Alloy, Anti-microbial
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polyethylene Terephthalate (PET)

Material Notes: Applications:
  • Gas equipment parts
Features:
  • Good anti-microbial
  • Warpageless
  • Flame resistant

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³ASTM D792
Water Absorption 0.060 %0.060 %24 hrs at 23°C; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 3.00 mm
0.0040 in/in
@Thickness 0.118 in
MD
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 3.00 mm
0.0090 in/in
@Thickness 0.118 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ASTM D785
Tensile Strength at Break 142 MPa20600 psiASTM D638
Elongation at Break 1.8 %1.8 %ASTM D638
Flexural Strength 170 MPa24700 psiASTM D790
Flexural Modulus 8.50 GPa1230 ksiASTM D790
Izod Impact, Notched 0.650 J/cm1.22 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 24.0 kV/mm
@Thickness 2.00 mm
610 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 90 sec90 secTungsten electrode; ASTM D495
Comparative Tracking Index 175 - 249 V175 - 249 VIEC Pub1.112, class 3; IEC Method
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 µm/m-°C
@Temperature 20.0 °C
19.4 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 205 °C401 °FBall pressure temperature; ASTM UL746B
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 265 °C509 °FMolding temperature
Mold Temperature 80.0 °C176 °F
Drying Temperature 140 °C284 °F
Dry Time 3 hour3 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC605P PBT/PET Alloy, Anti-microbial
Aclo Acculoy POL063L Polycarbonate PET Alloy
Toyobo VYLOPET® EMC320R Polyester Resin
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant

PTOY659 / 70819

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.