MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding performance. CHO-SHIELD® 2040’s robust formulation can be applied in both high and low volume paint application. CHO-SHIELD® 2040 is ideal for use on electronic enclosures and assemblies. CHO-SHIELD® 2040’s composition allows for simple, standard application using conventional equipment with minimal dry-time and handling. CHO-SHIELD® 2040 is ideal for use on medical electronic enclosures and assemblies which require high level, reliable EMI shielding performance and may benefit from silver’s antimicrobial properties.

Application: Superior EMI shielding, Anti-static protection, Surface grounding, Coating of ABS, PC/ABS, and many other types of plastic enclosures.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.50 g/cc1.10 - 1.50 g/ccASTM D792
Solids Content 42 %42 %
Volatile Organic Compounds (VOC) Content 741 g/l741 g/l
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.025 ohm
@Thickness 0.0250 mm
<= 0.025 ohm
@Thickness 0.000984 in
Shielding Effectiveness  73 dB
@Frequency 1e+10 Hz
73 dB
@Frequency 1e+10 Hz
 >= 75 dB
@Frequency 10000 - 8.00e+7 Hz
>= 75 dB
@Frequency 10000 - 8.00e+7 Hz
 80 dB
@Frequency 1e+8 Hz
80 dB
@Frequency 1e+8 Hz
 85 dB
@Frequency 1e+9 Hz
85 dB
@Frequency 1e+9 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Dry Time  10 - 20.0 hour
@Temperature 24.0 °C
10 - 20.0 hour
@Temperature 75.2 °F
then 30 minutes at 65°C
 24.0 hour
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Full Dry
Tack-Free Time 30.0 min
@Temperature 24.0 °C
0.500 hour
@Temperature 75.2 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Adhesion5BASTM D 3359
Coverage267 sq ft/galat 0.001 in
FillerSilver
PolymerAcrylic
Suggested Spraying Viscosity #2 Zahn Cup16 - 22 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUCON TR1000 PMMA+CNT
Trinseo Plexiglas® VS-UVT Acrylic
Overview of materials for Styrene Acrylonitrile (SAN), Transparent
Asahi Kasei Delpet® 670N Acrylic Molding Compound

PCHOME230 / 130940

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.