MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® R 500/60 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 500/60 is a peroxide curing HCR silicone rubber for general purpose applications.

Special features:

  • good mechanical properties
  • great filler acceptance
  • heat stability with stabilizers ELASTOSIL® AUX STAB HX
Application: Technical molding and extrusion applications.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1 A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60curing agent E; DIN 53505
 61curing agent C1; DIN 53505
Tensile Strength at Break 10.7 MPacuring agent E; DIN 53504 S1
 10.9 MPacuring agent C1; DIN 53504 S1
Elongation at Break 470 %curing agent E; DIN 53504 S1
 510 %curing agent C1; DIN 53504 S1
Tear Strength 26.0 kN/mcuring agent C1; ASTM D624 B
 26.0 kN/mcuring agent E; ASTM D624 B
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Treatment Temp. 135 °C
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3842/60 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R 427/70 High Strength Silicone Base
Wacker Elastosil® R 402/60 US Silicone Rubber
Wacker Elastosil® R 402/60 Silicone Rubber
Wacker Elastosil® R 401/70 Silicone Rubber

PWACK9212 / 204741

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.