MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem AKROFORM® MBTS-75/EPR/P Polymeric Dispersion
Categories: Other Engineering Material

Material Notes: Product Description: Akroform MBTS-75/EPR/P is a 75% dispersion of MBTS in a polymeric binder. MBTS is the most widely used organic accelerator. It is very active at temperatures above 280°F. MBTS requires the presence of zinc oxide, fatty acid and sulfur for optimal performance. It is activated by aldehyde amines, dithiocarbamates, alkaline and basic materials; in general, guanidines and thiurams. MBTS is also used as a retarder in non-sulfur modified polychloroprene cure systems and is a potent retarder in peroxide cures. To retard a peroxide-cured EPDM, add 0.25-0.50 phr MBTS and 1.0-2.0 phr TAC coagent to slow scorch but maintain state-of-cure. MBTS is a reasonably safe processing accelerator, but increased scorch resistance can be obtained by using Retarder PX, Retarder AK, or Retarder SAFE. MBTS can also be used as a mild peptizer for natural rubber.

Chemical Dispersions: Polymer bound or encapsulated dispersions are a proven means of upgrading plant safety, efficiency, quality & raw material control. Akrochem polymer bound or encapsulated dispersions eliminate any irritating dust, as well as other potential hazards in handling powders in the plant. The physical form is easy to handle and weigh accurately. As a dispersion, better uniformity of the mix at low process temperatures are possible.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/cc
 
Thermal PropertiesMetricEnglishComments
Melting Point 174 °C345 °Ffor active MBTS
 
Descriptive Properties
AppearanceOff-white to light yellow pellets
BinderEthylene Propylene Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH062 / 314980

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.