MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Saflex® 5/16" (22 mm) Laminated Insulating Units (Monolithic Glass - Air Space - Laminated Glass (inboard)
Categories: Ceramic; Glass

Material Notes: 1/4" LAG30[1/2" A.S.]1/8"

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 61 %Solar
 80 %Visible
UV Transmittance <= 0.00 %
 
Descriptive Properties
OITC31
Relative Heat Gain164 BTU/h-ft2-°F
Shading Coefficient0.79
Solar Heat Gain Coefficient0.68
STC37
U factor0.47 BTU/h-ft2-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Cyrolon® AR Polycarbonate Sheet
Eastman Saflex® 1" (25 mm) Laminated Insulating Units (Monolithic Glass - Air Space - Laminated Glass (inboard)
Eastman Saflex® 1" (26 mm) Laminated Insulating Units (Monolithic Glass - Air Space - Laminated Glass (inboard)
Eastman Saflex® 1" (26 mm) Double Laminated IGU (Laminated Glass - Air Space - Laminated Glass), LAG30
EnviroBrass® (SeBiLOY®) I Lead-Free Casting Alloy, UNS C89510

PEAT7037 / 183605

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.