MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Akrochem AKROWAXES™ 135 Paraffin
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: AKROWAX 135 Synthetic Paraffin is a mixture of linear and branched paraffinic hydrocarbons. It is designed for use in the rubber articles as a viscosity modifier, gelling agent, slip agent, and protectorant. Typical loadings are 2 to 4 phr in a normal applications; 4 to 8 phr in highly loaded compounds. Akrowax 135 does not produce a wax film bloom as “thick” as regular paraffin waxes. This wax complies with F.D.A. Regulations for use as indirect or direct food additives described in Code of Federal Regulations, Title 21, Chapter 1, Section 172.886 and 178.3710 as well as 177.2600, Rubber Articles Intended For Repeated Use.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.770 g/cc
 
Mechanical PropertiesOriginal ValueComments
Penetration 24Needle
 
Thermal PropertiesOriginal ValueComments
Melting Point 56.7 - 58.3 °CCongealing Point; ASTM D938
Dropping Point 141 °FASTM D127
 
Descriptive Properties
AppearanceWhite Solid
Color>+26Saybolt, ASTM D156

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH631 / 315549

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.