MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Clyrell RC 549S Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: The specialty polypropylene Clyrell product portfolio includes random and impact copolymers based on Ziegler-Natta catalysts. Clyrell RC549S is a clarified development polypropylene resin with antistatic additivation used in injection molding. It features an excellent combination of high stiffness and high transparency that enables customers to achieve excellent organoleptic performance and a superior aesthetic appearance which appeals to end users. Applications: Clear Containers, House wares, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1133-1
Melt Flow 44 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 34.0 MPaISO 527-1,-2
Elongation at Break >= 50 %ISO 527-1,-2
Elongation at Yield 10 %ISO 527-1,-2
Tensile Modulus 1470 MPaISO 527-1,-2
Charpy Impact, Notched 1.20 kJ/m²
@Temperature 0.000 °C
Type 1, Edgewise, Notch A; ISO 179
 2.50 kJ/m²
@Temperature 23.0 °C
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 86.0 °Cunannealed; ISO 75B-1,-2
 
Optical PropertiesOriginal ValueComments
Haze 10 %
@Thickness 1.00 mm
injection molded disc; ASTM D1003
Gloss 128 %@ 60°; ASTM D 2457
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem RP250 Polypropylene Random Copolymer
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade
LyondellBasell Hostacom PP HH42L 356015 Polypropylene
Borealis BJ356MO Polypropylene Copolymer
Borealis BE375MO Polypropylene Copolymer

PEQT7077 / 218715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.