MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ITW Insulcast® INSULCAST 116 FR Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST 116 FR is a one to one ratio (weight or volume) epoxy potting and casting compound designed for production use. The convenient mixing ratio of the material makes it ideal for production line mixing as well as automatic dispensing. INSULCAST 116 FR is among the safest epoxy compounds available. It appreciably reduces the risk of eye, skin or respiratory problems generally associated with the use of epoxy compounds.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccpart B. Uncured
 1.50 g/ccpart A. Uncured
Viscosity 7200 cPPart A; ASTM D2393
 8100 cPmixed. Uncured
 11000 cPPart B; ASTM D2393
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength 9500 psiASTM D638
Elongation at Break 8.0 %cured; ASTM D638
Flexural Strength 10000 psiASTM D790
Compressive Strength 12500 psiASTM D695
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 4.4
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 420 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
Thermal Conductivity 0.432 W/m-K
Maximum Service Temperature, Air 105 °C
Heat Distortion Temperature 70.0 °CLoad Not Reported
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 22.0 °C
accelerated. Then 2 hours @ 130°F
 16.0 - 24.0 hour
@Temperature 22.0 °C
Pot Life 90.0 min100 gram mass
Gel Time 180 - 240 min
@Temperature 25.0 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorBlackpart A. Uncured
 neutralpart B. Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9088 / 239598

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.