System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Durethan® AKV 25 FN00 000000 Nylon 66 (PA66), 25% Glass Fiber Reinforced, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
PA 66, 25% glass fibers, injection molding, halogen free flame retardant
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Bulk Density
0.700
g/cc
ISO 60
Density
1.39
g/cc
ISO 1183
Moisture Absorption at Equilibrium
1.5 %
50% RH; ISO 62
Water Absorption at Saturation
4.6 %
ISO 62
Linear Mold Shrinkage, Flow
0.0030
cm/cm
60x60x2; 270 °C / WZ 120°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0090
cm/cm
60x60x2; 270 °C / WZ 120°C; 600 bar; ISO 294-4
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 270 °C
ISO 1133-1
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
125
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
3.0 %
5 mm/min; ISO 527-1,-2
3.4 %
50 mm/min, Nominal; ISO 527-1,-2
Tensile Modulus
9600
MPa
1 mm/min; ISO 527-1,-2
Flexural Strength
210
MPa
2 mm/min; ISO 178-A
Flexural Modulus
9100
MPa
2 mm/min; ISO 178-A
Flexural Strain at Break
3.3 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
55.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
60.0
kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
60.0
kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
Charpy Impact, Notched
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
Electrical Properties
Original Value
Comments
Volume Resistivity
7.40e+13
ohm-cm
IEC 60093
Surface Resistance
1.10e+16
ohm
IEC 60167
Dielectric Strength
35.0
kV/mm
@Thickness 1.00 mm
IEC 60243-1
Comparative Tracking Index
0.00
V
Solution A; UL 746A
600
V
Solution A; IEC 60112
Thermal Properties
Original Value
Comments
Melting Point
260
°C
10°C/min; ISO 11357-1,-3
Maximum Service Temperature, Air
228
°C
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi)
225
°C
ISO 75-1,-2
Vicat Softening Point
225
°C
@Load 5.10 kg
120°C/h; ISO 306
Flammability, UL94
V-0
@Thickness 0.400 mm
V-0
@Thickness 0.750 mm
V-0
@Thickness 1.50 mm
V-0
@Thickness 3.00 mm
Oxygen Index
38 %
Method A; ISO 4589-2
Glow Wire Ignition Temperature
775
°C
@Thickness 0.400 mm
IEC 60695-2-13
775
°C
@Thickness 0.750 mm
IEC 60695-2-13
775
°C
@Thickness 1.50 mm
IEC 60695-2-13
775
°C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index
960
°C
@Thickness 0.400 mm
IEC 60695-2-12
960
°C
@Thickness 0.800 mm
IEC 60695-2-12
960
°C
@Thickness 1.50 mm
IEC 60695-2-12
960
°C
@Thickness 3.00 mm
IEC 60695-2-12
Shrinkage, MD
0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, 60x60x2; ISO 294-4
Shrinkage, TD
0.10 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, 60x60x2; ISO 294-4
Processing Properties
Original Value
Comments
Melt Temperature
270
°C
injection molding; ISO 294
265
-
285
°C
Mold Temperature
80.0
°C
injection molding; ISO 294
80.0
-
100
°C
Drying Temperature
80.0
°C
Dry Time
2.00
-
6.00
hour
Moisture Content
0.030 - 0.070 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Envalior Durethan® BKV 25 FN01 000000 Nylon 6 (PA6), 25% Glass Fiber Reinforced, Dry
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled
BASF Ultramid® A3HG5 25% Glass Filled PA66 (Dry)
Envalior Durethan® AKV 25 F30 000000 Nylon 66 (PA66), 25% Glass Fiber Reinforced, Dry
Overview of materials for Nylon 66, 30% Glass Fiber Filled
PLANW9210 / 208007
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.