MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 6202 Styrene-Acrylic Resin Solution
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Rovene® 6202 is a solution version of Rovene® 6201 solid styrene-acrylic resin neutralized with ammonia hydroxide. It can be used as a pigment dispersant resin and as a modifying additive in inks or overprint varnishes. Rovene® 6202 is a general use resin solution that is used as a grinding resin to produce pigment dispersions. The solution can also be used as an additive to modify certain properties of an ink or overprint varnish. The addition of Rovene® 6202 will increase gloss, increase block resistance and improve resolubility on press. The solution can also be crosslinked due to the carboxyl functionality of the styrene-acrylic resin.

Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6202 Material Safety Data Sheet before handling, storing, or using this product.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 68 - 70 %
pH 8.1 - 8.8
Molecular Weight 7000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 218[mgKOH/g]
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMCP134 / 157411

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.