MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ashley Polymers Ashlene® P1081 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: A high viscosity resin for blow molding as well as injection molding heavy wall parts requiring maximum impact strength. Also available: P1083, same with UV stabilizer; P1081R, same with release; P1083R, with UV and release; P1084, FDA approved.

Data provided by the manufacturer

Key Words: PC; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
Moisture Absorption at Equilibrium 0.35 %0.35 %ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm0.0060 in/inASTM D955
Melt Flow 3.0 - 4.0 g/10 min3.0 - 4.0 g/10 minCond. O
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7070ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Ultimate 66.0 MPa9570 psiATSM D638
Elongation at Break 125 %125 %ASTM D638
Elongation at Yield 8.0 %8.0 %ASTM D638
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® Rx2430 Polycarbonate
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant
LG Chemical Lupoy 3010-10 Polycarbonate Resin
LG Chemical Lupoy 1200-03 Polycarbonate Resin
Covestro Makrolon® 2408 Polycarbonate

PNAC56 / 54642

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.