MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Alathon® L5045 High Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Applications
ALATHON L 5045 is a medium molecular weight high density polymer for use in blown film extrusion applications. Typical applications include millinery bags, coextrusions and plastic netting.

Regulatory Status
L 5045 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing L 5045 can only be made when the processing conditions, equipment and end use are known.

Typical Extrusion Condtions: BUR=2-2.5:1; Frost Line 24 inch; 1.0 Mil Film; Melt Temperature- 390-420°F(199-216°C)

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ASTM D792
Thickness 25.4 microns1.00 mil2 - 2.5 BUR; Frost line 24 inch
Melt Flow 0.45 g/10 min0.45 g/10 minASTM D1238
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 216 °C390 - 421 °FTypical Extrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Braskem HM 150 HDPE Monofilament Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Chase Plastics CP Pryme® PE200-HD20M General Purpose High Density Polyethylene
Dow DOWLEX™ IP-10 High Density Polyethylene

PEQU0137 / 36566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.