MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

RAMPF RAKU® TOOL FM-7080 Polyurethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Rigid polyurethane foam

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
Applications:
  • For hand-batch and meter-mix processing
Cure: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 - 0.176 g/cc0.00462 - 0.00636 lb/in³Cure; ASTM D-792
 1.16 g/cc0.0419 lb/in³Hardener; ASTM D-792
 1.20 g/cc0.0434 lb/in³Resin; ASTM D-792
Viscosity 100 cP100 cPResin; ASTM D-2393
 250 cP250 cPMix; ASTM D-2393
 675 cP675 cPHardener; ASTM D-2393
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1.33 - 1.67 min0.0222 - 0.0278 hourRise time
 1.92 - 2.25 min0.0319 - 0.0375 hourTack Free time
 10.0 - 20.0 min0.167 - 0.333 hourDemold
 
Descriptive Properties
ColorLight Tan
Mix Ratio100:100Resin: Hardener, Volume
 100:97Resin: Hardener, Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF154 / 317754

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.