MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay RHODAFAC® ASI-80 Octyl phosphonic acid
Categories: Fluid

Material Notes: Identification: ALKYL PHOSPHONATE DERIVATIVE

CAS: 4724 – 48 – 5

EINECS: 225 – 218 – 5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Corrosion inhibitor for ferrous metals, aluminum, zinc, magnesium and their alloys. Effective in alkaline water based formulations such as metal working fluids and cleaning formulations. Dispersant for metal powders and oxides.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Solids Content 78 - 82 %78 - 82 %OPTI067
pH 2.32.35% solution
Viscosity 85 cP85 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point 10.0 °C50.0 °FFreezing Point
 
Processing PropertiesMetricEnglishComments
Moisture Content 9.0 - 11 %9.0 - 11 %OSTM074
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceColorless mobile liquid
Assay>96 mol%OPTI064
Color<50Hazen, 80% solution in 10% water/10% ethanol, OSTM030
CompositionEthanol9-11%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Rhodafac ASI 30 SOLUTION OF OCTYL PHOSPHONIC ACID IN WATER
Solvay RHODAFAC® ASI-100 Octyl phosphonic acid

WRHOD423 / 137654

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.