MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 8560S Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 8560S adhesive is a general purpose, one-coat aqueous (water-based) adhesive used to bond a wide variety of vulcanized and unvulcanized rubber compounds to metal. A single coat of Chemlok 8560S adhesive will bond compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR) and nitrile (NBR) polymers to a variety of metals such as carbon and alloy steels, stainless steel and aluminum during the vulcanization process. Chemlok 8560S adhesive has been formulated using water as the carrier system and does not contain co-solvents. When environmental conditions are severe, Chemlok 8560S adhesive is recommended to be used over Chemlok 8007 water-based primer.

Features: serves as a post vulcanization (cured rubber) bonding agent capable of bonding a wide variety of vulcanized rubber compounds. requires only a single coat for most applications, reducing labor, inventory and shipping costs. uses water for dilution; has low VOC emissions.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 - 1.22 g/cc0.0424 - 0.0442 lb/in³
Solids Content 38 - 42 %38 - 42 %by weight
Brookfield Viscosity 50 - 250 cP
@Temperature 25.0 °C
50 - 250 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm, Zahn Cup #2
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month
@Temperature 21.0 - 27.0 °C
3.00 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
pH6 to 8
SolventsDeionized Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9022 / 232411

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.