MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Destech Open-Celled Glassy Carbon Foam
Categories: Carbon; Other Engineering Material; Composite Core Material

Material Notes: Destech glassy (vitreous) carbon foam is available in different grades depending on the number of pores per inch (ppi). Standard grades are 10, 45, 100 and 500 ppi. Custom grades are available on a special order basis.

Areas of applications include filtration, electrochemical cells, heating elements, electrodes, fuel cells, acoustics, high temp insulation, foam cores. Data provided by the manufacturer, Destech Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.0190 - 0.390 g/ccDependent on grade.
Density 1.50 g/ccLigament density. Dependent on grade.
Open Porosity >= 90 %Closed porosity 0%.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.300 - 7.00 MPaDependent on grade
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0750 ohm-cmDependent on grade.
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.60 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.100 - 0.900 W/m-KDependent on grade and temperature.
Maximum Service Temperature, Air 300 °C
Maximum Service Temperature, Inert 3000 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Graphite, Carbon, C
BACT DLC Diamond-Like Coating
Cancarb Thermax® Floform N990 Medium Thermal Carbon Black
Cancarb Thermax® Powder N991 Ultra-Pure Medium Thermal Carbon Black
Carlisle 201HD Carbon-Carbon Composite

CDC001 / 769

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.