MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Park Aerospace Nelcote® S-860 Silicone Prepreg, 1581-112NPH E-Glass Reinforced
Categories: Polymer; Thermoset; Silicone

Material Notes: Nelcote® S-860 is a MIL-P-25518 type silicone resin with a good combination of electrical and high temperature properties. GMS4001 qualified specifications

Key Features and Benefits:

  • 500°F maximum service temperature
  • Good electrical and mechanical properties at high temperatures
  • Low out-gassing for space applications

Applications/Qualifications:

  • Radomes
  • Aircraft Structures

Information provided by Park Electrochemical Corp.

Key Words: SI
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³
Volatiles <= 2.5 %
@Temperature 163 °C
<= 2.5 %
@Temperature 325 °F
8 min
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5959
Tensile Strength, Yield 221 MPa
@Temperature 23.9 °C
32000 psi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Tensile Modulus 18.6 GPa
@Temperature 23.9 °C
2700 ksi
@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Flexural Strength 283 MPa
@Temperature 23.9 °C
41000 psi
@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 18.6 GPa
@Temperature 23.9 °C
2700 ksi
@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 165 MPa
@Temperature 23.9 °C
24000 psi
@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 19.3 GPa
@Temperature 23.9 °C
2800 ksi
@Temperature 75.0 °F
Dry; ASTM D695
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.15
@Frequency 9.375e+9 Hz
4.15
@Frequency 9.375e+9 Hz
Dissipation Factor 0.013
@Frequency 9.375e+9 Hz
0.013
@Frequency 9.375e+9 Hz
 
Processing PropertiesMetricEnglishComments
Gel Time 3.00 - 4.00 min3.00 - 4.00 min
Shelf Life  3.00 Month
@Temperature 4.44 °C
3.00 Month
@Temperature 40.0 °F
 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)302
Prepreg Resin Content (%)31-41
Resin Flow (%)10-16340°F, 10psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
E-CRGlas® Fiber
AGY ADVANTEX® Generic Glass Fiber
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
Park Aerospace Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced

PPARK069 / 89341

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.