MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rogers Arlon A3020-B004-12 Silicone Rubber/Fiberglass Laminate  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Side 1: cured fusible silicone rubber; Substrate: 25% sinusoidal fiberglass; Side 2: cured fusible silicone rubber; Interleave: 1 mil PE film

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccsilicone property; Arlon SQA-TMS-024
Thickness 152 microns6.00 milside 1; Arlon SQA-TMS-003
 152 microns6.00 milside 2; Arlon SQA-TMS-003
 203 microns8.00 milsubstrate; Arlon SQA-TMS-003
 508 microns20.0 miloverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050silicone property; ASTM D2240
Tensile Strength at Break 0.414 MPa60.0 psiASTM D624
Tensile Strength, Ultimate 8.27 MPa1200 psisilicone property; ASTM D412
Elongation at Break 415 %415 %silicone property; ASTM D412
Elongation at Yield 31 %31 %ASTM D412
Adhesive Bond Strength 0.0414 MPa6.00 psiArlon SQA-TMS-047
Tear Strength 15.8 kN/m90.0 pliDie B; silicone property; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 28.1 kV/mm715 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 23.9 °C
12.0 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 55096R028 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51106R015 Silicone Rubber/Fiberglass Laminate
Rogers Arlon 51106R020 Silicone Rubber/Fiberglass Laminate

PARL049 / 79701

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.