System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LG Chemical LUPOL GP1007FE Flame Retardant PP
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Flame Retardant
Material Notes:
Description: Injection Molding, FR PP, General Purpose, Flame Retardant
Application: Electrical & Electronic, Automotive Parts
CAS: 9003-07-0 and 1309-64-4
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.930
g/cc
0.930
g/cc
ASTM D792
Maximum Moisture Content
0.020
0.020
Injection Molding
Linear Mold Shrinkage, Flow
0.016
-
0.018
cm/cm
@Thickness 3.20 mm
0.016
-
0.018
in/in
@Thickness 0.126 in
ASTM D955
Melt Flow
1.5
g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
25.5
MPa
@Thickness 3.20 mm
3700
psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break
>= 200 %
@Thickness 3.20 mm
>= 200 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength
29.4
MPa
@Thickness 6.40 mm
4270
psi
@Thickness 0.252 in
10mm/min; ASTM D790
Flexural Modulus
0.981
GPa
@Thickness 6.40 mm
142
ksi
@Thickness 0.252 in
10mm/min; ASTM D790
Izod Impact, Notched
>=
4.90
J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
>=
9.18
ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Electrical Properties
Metric
English
Comments
Arc Resistance
120
-
180
sec
120
-
180
sec
ASTM D495
Hot Wire Ignition, HWI
7.0
-
15
sec
@Thickness >=0.750 mm
7.0
-
15
sec
@Thickness >=0.0295 in
15
-
30
sec
@Thickness >=1.50 mm
15
-
30
sec
@Thickness >=0.0591 in
30
-
60
sec
@Thickness >=3.00 mm
30
-
60
sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness 0.750 mm
>=
120
arcs
@Thickness 0.0295 in
>=
120
arcs
@Thickness 1.50 mm
>=
120
arcs
@Thickness 0.0591 in
>=
120
arcs
@Thickness 3.00 mm
>=
120
arcs
@Thickness 0.118 in
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
110
°C
@Thickness 3.20 mm
230
°F
@Thickness 0.126 in
Unannealed; ASTM D648
UL RTI, Electrical
65.0
°C
@Thickness >=0.750 mm
149
°F
@Thickness >=0.0295 in
120
°C
@Thickness >=1.50 mm
248
°F
@Thickness >=0.0591 in
120
°C
@Thickness >=3.00 mm
248
°F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact
65.0
°C
@Thickness >=0.750 mm
149
°F
@Thickness >=0.0295 in
120
°C
@Thickness >=1.50 mm
248
°F
@Thickness >=0.0591 in
120
°C
@Thickness >=3.00 mm
248
°F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact
65.0
°C
@Thickness >=0.750 mm
149
°F
@Thickness >=0.0295 in
120
°C
@Thickness >=1.50 mm
248
°F
@Thickness >=0.0591 in
120
°C
@Thickness >=3.00 mm
248
°F
@Thickness >=0.118 in
Flammability, UL94
V-2
@Thickness >=0.750 mm
V-2
@Thickness >=0.0295 in
V-2
@Thickness >=1.50 mm
V-2
@Thickness >=0.0591 in
V-2
@Thickness >=3.00 mm
V-2
@Thickness >=0.118 in
Processing Properties
Metric
English
Comments
Zone 1
230
-
245
°C
446
-
473
°F
Extrusion Molding
Zone 2
200
-
230
°C
392
-
446
°F
Extrusion Molding
Zone 3
220
-
240
°C
428
-
464
°F
Extrusion Molding
Zone 4
220
-
240
°C
428
-
464
°F
Extrusion Molding
Die Temperature
220
-
240
°C
428
-
464
°F
Extrusion Molding
Melt Temperature
230
-
245
°C
446
-
473
°F
Extrusion Molding
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Injection Molding
Dry Time
3.00
-
5.00
hour
3.00
-
5.00
hour
Injection Molding
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
LG Chemical LUPOL GP1007F Flame Retardant PP
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact
LG Chemical LUPOL GP2150 PP+GF15%
PLAY459 / 148469
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.