MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

HB Fuller KALAR® 5281 Elastomer
Categories: Polymer; Thermoplastic

Material Notes: KALAR® 5281 is a partially cross-linked butyl rubber compound pelletized for easy handling. KALAR® 5281 is modified with ethylene vinyl acetate (EVA) copolymer to improve lower temperature toughness and higher temperature processing. KALAR® products feature all the performance attributes expected of butyl rubber. KALAR® 5281 is light amber to yellow in color and is among the tightest cross-linked butyl rubber of the KALAR® products. It is designed as the starting point for applications that require the maximum resistance to creep and slump.

Features and Benefits: KALAR® 5281 contains no filler and its tenacity is due to the degree of cross-linking; not reinforcing fillers. This feature permits the compounder the widest formulating latitude. Other key performance benefits include:

  • Elimination of butyl rubber pre-mastication
  • Pellets may be metered to facilitate mixing
  • Requires no vulcanization
  • Readily acceptable in a wide range of solvents
  • Extends with high levels of fillers and plasticizers
  • Compatible with a wide choice of compounding ingredients
  • Creep and cold-flow resistance
  • Compounding economy

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D71
Density 0.923 g/cc0.0333 lb/in³ASTM D71
Mooney Viscosity 70 - 83
@Temperature 127 °C
70 - 83
@Temperature 261 °F
ASTM D1646
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAmber
ConsistencyRubber Pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL239 / 317030

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.