MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4)  (discontinued **)
Categories: Ceramic; Nitride

Material Notes: Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten metals. This lower cost alternative to the fully dense silicon nitride grades can be manufactured to close tolerance without the need for expensive diamond grinding.

Features:

  • Strength
  • Hertzian Contact Strength
  • Structural Reliability
  • Net Shape Fabrication

Applications:

  • Automotive Components
  • Bearings
  • Wear Components
  • Logging Tools
  • Drilling components
  • Measuring wheels
  • Electrical Insulators
  • Seal rings

Information provided by Ceradyne, Inc.

Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.20 g/cc
Porosity 0.00 %
Weibull Modulus 15 - 50
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1450HV (0.3); kg/mm2
Abrasive Hardness 825Abrasive Wear Resistance Parameter
Modulus of Elasticity 310 GPa
Flexural Strength 700 - 800 MPa
Poissons Ratio 0.27
Fracture Toughness 6.00 MPa-m½
Shear Modulus 122 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cm
Dielectric Constant 8.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.10 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 26.0 W/m-K
 
Descriptive Properties
Purity, %92
Theoretical Density, %>99.5
Thermal Shock Parameter, °C610

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ceradyne Ceralloy® 147-1B Reaction Bonded Silicon Nitride (Si3N4)
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4)
Silicon Nitride, reaction sintered

CCERDN42 / 720

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.