MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Sheet BFG Thermally Conductive Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Silicone

Material Notes: TRA-SHEET BFG is a thermally conductive and insulated silicone sheet with glass fiber reinforcement. It is suitable for heat dissipation applications for high power devices. It has been utilized successfully to transfer heat away from an active device to a heat spreader or heat sink.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/cc
Thickness 300 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.40e+15 ohm-cm
Dielectric Constant 3.6
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 4.10 W/m-K
Flammability, UL94 V-0
 
Descriptive Properties
Color White
Outgassing, NASA Passes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.75 PHR Sulfur
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 78 P 4766 NM Ether-Based TPU-For Cable Industry

PTRAC216 / 71144

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.