MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ascend Performance Materials Starflam® PX07037 PA6, Flame Retardant, Injection Molded
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Starflam PX07037 is an Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (IR laser marking grade)

Former Eurostar product. Eurostar has been acquired by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³DAM; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 74.0 MPa10700 psiDAM; ISO 527-2
Elongation at Break 7.3 %7.3 %DAM; ISO 527-2
Flexural Strength 95.0 MPa13800 psiDAM; ISO 178
Flexural Modulus 2.80 GPa406 ksiDAM; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 
Electrical PropertiesMetricEnglishComments
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secPLC 3; UL 746
 30 - 60 sec30 - 60 secPLC 2; UL 746
 30 - 60 sec30 - 60 secUL 746
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 >= 120 arcs>= 120 arcsPLC 0; UL 746
 
Thermal PropertiesMetricEnglishComments
UL RTI, Electrical  120 °C
@Thickness 0.750 mm
248 °F
@Thickness 0.0295 in
UL 746
 120 °C
@Thickness 1.60 mm
248 °F
@Thickness 0.0630 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.750 mm
149 °F
@Thickness 0.0295 in
UL 746
 75.0 °C
@Thickness 1.60 mm
167 °F
@Thickness 0.0630 in
UL 746
 75.0 °C
@Thickness 3.00 mm
167 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  85.0 °C
@Thickness 0.750 mm
185 °F
@Thickness 0.0295 in
UL 746
 85.0 °C
@Thickness 1.60 mm
185 °F
@Thickness 0.0630 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
Glow Wire Ignition Temperature  725 °C
@Thickness 0.750 mm
1340 °F
@Thickness 0.0295 in
IEC 60695-2-13
 750 °C
@Thickness 1.60 mm
1380 °F
@Thickness 0.0630 in
IEC 60695-2-13
 750 °C
@Thickness 3.00 mm
1380 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 250 °C464 - 482 °FInjection
Middle Barrel Temperature 250 - 260 °C482 - 500 °FInjection
Front Barrel Temperature 250 - 270 °C482 - 518 °FInjection
Melt Temperature 250 - 270 °C482 - 518 °FInjection
Mold Temperature 50.0 - 90.0 °C122 - 194 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesBromine Free
 Flame Retardant
 Halogen Content, None
 Laser Markable
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEUROSTA26 / 172040

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.