MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Celanese Vandar® 4602ZHR PBT, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: 4602ZHR is an unfilled hydrolysis resistant PBT alloy with excellent thermal stability, toughness and weatherability characteristics.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.017 - 0.022 cm/cm0.017 - 0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.022 cm/cm0.017 - 0.022 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 34.5 MPa5000 psiASTM D638
Tensile Strength, Yield 40.0 MPa5800 psi50mm/min; ISO 527-2/1A
Elongation at Break 180 %180 %50mm/min; ISO 527-2/1A
 180 %180 %ASTM D638
Elongation at Yield 6.0 %6.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 1.50 GPa218 ksi50mm/min; ISO 527-2/1A
Flexural Strength 45.0 MPa6530 psiISO 178
 49.0 MPa7100 psiASTM D790
Flexural Modulus 1.40 GPa203 ksiISO 178
 1.52 GPa220 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Izod Impact, Notched (ISO) NBNBISO 180/1A
Charpy Impact, Notched NBNBISO 179/1eA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vandar® 8000 PBT, Unfilled
Celanese Vandar® 6000 PBT, Unfilled
Celanese Vandar® 4602Z PBT, Unfilled
Celanese Vandar® 2500 PBT, Unfilled
Celanese Vandar® 2122 PBT, 10% Mineral Reinforced

PHCQ478 / 178933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.