MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Evonik ULTRASIL® VN 3 GR Silica
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: ULTRASIL® VN 3 GR as a precipitated silica is used as a reinforcing filler in all kind of rubber applications.

Properties and applications: ULTRASIL® VN 3 GR is a mechanically compacted granulate. On account of the granulation process it leads to less dust development during mixing. ULTRASIL® VN 3 GR has a high reinforcing potential and imparts to rubber compounds particularly high Shore hardness, tensile strength, tear resistance and abrasion resistance. In order to achieve optimum rubber-technical data the addition of activators like glycols, amines or other alkaline accelerators is necessary. On account of the higher surface area ULTRASIL® VN 3 can provide vulcanizates of excellent transparency.

Application fields are: Tires, mechanical rubber goods, cables and shoe soles of all kinds.

CAS No: 112926-00-8 and 7631-86-9

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.280 g/cc0.0101 lb/in³Poured; ASTM D1513
Particle Size <= 75 µm<= 75 µm<10% SA Ro-Tap; ISO 5794-1F
 >= 300 µm>= 300 µm>80% SA Ro-Tap; ISO 5794-1F
pH 6.26.25% in water; ISO 787-9
Specific Surface Area 167 m²/g167 m²/gCTAB; ISO 5794-1G
 180 m²/g180 m²/gN2; ISO 9277
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Fe (Iron) <= 400 ppm<= 400 ppm
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 97 %>= 97 %based on ignited substance (2 h/1000°C); ISO 3262-19
 
Descriptive Properties
Content<6 ppmMn
 <6 ppmCu
Electrical conductivity<1300 µS/cm4% in water, ISO 787-14
Loss on drying0.0552 hrs at 105°C, ISO 787-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIN021 / 317055

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.